图片名称

30 Concrete Questions The Basics You Need to Know

2026-11-10


 

1. What should be done when raw materials cannot be taken out of use immediately and concrete supply cannot be interrupted?

While contacting the raw-material supplier, assign dedicated personnel to control mixing-water quantities and monitor workability restoration at the jobsite, preventing workers from adding water on their own. If necessary, keep the water-to-binder ratio unchanged and appropriately increase the cement content to improve concrete flowability. In general, each 1 cm increase in slump requires a 1.5%–2.5% increase in cement-paste volume per cubic meter of concrete.

 

2. Can every type of fly ash be used in ready-mixed concrete?

Fly ash is classified as Grade I, II or III according to its fineness, water-demand ratio and carbon content. Grade I and Grade II fly ash can be used in ready-mixed concrete.

 

3. When is fly ash not advisable?

During winter construction, particularly at −10°C or below, fly ash is not advisable. Fly-ash concrete has relatively low early strength and needs a longer period of precuring above freezing to reach the critical strength required to resist early freezing. If site insulation is inadequate, the concrete is very susceptible to freezing damage. In addition, fly ash must not be used in concrete floors finished and troweled as they are placed, or in concrete subject to deicing-salt requirements.

 

4. Can the acceptance age for fly-ash concrete be extended?

Yes. Because fly ash contributes to later-age strength, China’s Technical Code for Application of Fly Ash Concrete (GB J146) specifies the recommended ages for the design strength grade of fly-ash concrete as follows: 28 days for above-ground works; 28 or 60 days for works at ground level; 60 or 90 days for underground works; and 90 or 180 days for mass concrete.

 

5. Under what conditions is silica fume used?

Silica fume is mainly used to produce high-strength concrete, sulfate-resistant concrete, chloride-resistant concrete, underwater concrete, concrete exposed to deicing salts, and highly abrasion-resistant pavement concrete.

 

6. When is zeolite powder used?

Zeolite powder can be used as an active mineral addition to cement.

Zeolite powder can replace part of the cement in concrete and improve water retention. In particular, when high dosages of polycarboxylate high-range water reducers are used to produce highly flowable or ultra-high-strength concrete, an appropriate amount of zeolite powder can effectively improve water retention and prevent bleeding.

In lightweight-aggregate concrete, the addition of zeolite powder increases the structural viscosity of the cement paste and can substantially reduce the tendency of lightweight aggregates to float during vibration and molding.

Zeolite-powder concrete is also suitable for underwater concrete and concrete cured in damp underground environments, offering good frost resistance and resistance to water penetration. When zeolite powder is used to produce high-performance concrete, a cement replacement level of 10% is preferable.

 

7. Why do some concretes made with naphthalene-based high-range water reducers have many surface bubbles after stripping, and what should be done?

Some admixture manufacturers purchase inexpensive crude naphthalene or mixed naphthalene. Normal naphthalene appears white or yellow, whereas naphthalene containing impurities appears pink or brick red. These impure materials have a high phenol content and low purity, introducing many air bubbles through the high-range water reducer. Poor-quality naphthalene can introduce 3% air into the concrete. The bubbles are relatively large and take longer to dissipate, directly affecting concrete strength. In this situation, contact the admixture manufacturer promptly and suspend use to avoid compromising concrete strength.

 

8. What precautions are needed when using air-entraining admixtures?

First, control the air content, generally within 2%–4% by volume; otherwise, concrete strength will decrease. Also, do not select poor-quality air-entraining admixtures that produce large bubbles with wide spacing, such as sodium dodecyl sulfonate or calcium lignosulfonate. Even a slightly excessive dosage can cause a substantial reduction in concrete strength. Before use, determine the appropriate product and dosage through testing.

 

9. How does excessive waiting time at the jobsite affect concrete quality?

Although a retarder is added to concrete, its retarding effect is limited. After more than two hours, cement begins to hydrate, slump starts to decrease, and some concrete strength is lost. Trials conducted by some concrete producers have shown that strength starts to decline when waiting time at the jobsite exceeds two hours. Therefore, concrete should not wait at the jobsite for more than two hours.

 

10. What happens when water is added to a concrete truck mixer?

The specified water-to-binder ratio gives concrete the required flowability and strength. Adding water afterward reduces strength because excess water leaves voids after evaporation, weakening the concrete cross-section. According to test data from some concrete producers, every additional 10 kg of water reduces 28-day strength by 3.7 MPa. Therefore, adding water to truck mixers at the jobsite must be strictly prohibited.

 

11. What should be done when concrete arrives with a slump too low for pumping?

The only option is to restore workability by redosing a concrete admixture. Adjust the dosage according to the slump of the concrete in the truck. Typical dosages are 0.5–1 kg/m³ for powdered admixtures and 1–2 kg/m³ for liquid admixtures. After addition, rotate the drum at high speed for about 1–2 minutes to restore workability. Repeated trials have shown that concrete can be replasticized repeatedly without a general loss of strength, provided no water is added and the holding time at normal temperature does not exceed two hours.

Because pumping admixtures may contain retarding and air-entraining components, adding them to concrete may cause delayed setting or reduced strength.

12. How long after placement does concrete reach initial and final set, and how can these be judged?

At normal temperature, concrete reaches initial set in 6–8 hours. Initial set is indicated when the surface is no longer sticky to a light touch, bleed water has receded, and a thin shiny film appears. Final set is reached when the surface turns pale and pressing it leaves no mark, typically after about 8–10 hours. These times become shorter or longer in summer and winter as temperature changes.

 

13. What is high-early-strength concrete?

At normal temperature, ordinary concrete reaches approximately 70% of its design strength at seven days and 100% at 28 days. When measures are taken to reach design strength in about 15 days to meet construction schedules or formwork reuse needs, it is called high-early-strength concrete. Concrete that reaches design strength in about seven days at normal temperature is called ultra-high-early-strength concrete.

Such concrete can generally be produced using an ultra-high-early-strength pumping admixture, by raising the specified concrete strength by two grades, or by using P.O 42.5R cement.

 

14. What should be considered when designing a mass-concrete mix?

Mass concrete must be protected against structural cracking caused by a core-to-surface temperature difference exceeding 25°C. Mix design should therefore address the following points:

大体积混凝土要防止其内外温差超过25℃而引起的结构裂缝,因此配合比设计时要注意以下几点:

Control cement content and select a cement with lower heat of hydration and slower setting, such as dam cement, portland slag cement or portland fly-ash cement.

Use fly ash and finely ground slag powder to reduce the heat of hydration.

Use a retarding water reducer or a high-range water reducer.

To lower the concrete placement temperature, use groundwater that meets mixing-water standards and, if necessary, add some ice.

 

15. How does temperature typically develop in mass concrete?

Mass concrete generally reaches its peak temperature two to three days after placement. For example, a 2 m thick foundation slab made with 360 kg/m³ of strength-class 42.5 cement, placed in summer at 32°C, may reach a core temperature of about 80°C. After four days, most of the hydration heat has been released and the internal temperature gradually falls. This elevated-temperature condition may continue for more than ten to over thirty days, and heat dissipation may take much longer in some hydraulic mass-concrete structures. Based on this pattern, temperature control should focus on the first week after placement, especially days two and three.

 

16. How does a high fly-ash content help suppress the peak temperature of concrete?

Fly ash helps lower the peak temperature of mass concrete and delay its occurrence. At fly-ash contents of 10%–50% by mass of binder, the three-day hydration peak is reduced by 5.9%–35.1%, and the temperature peak is delayed by 0.5–3.2 hours.

 

17. What should be checked when coarse and fine aggregates arrive at the plant?

For coarse aggregates, control particle size, grading, particle shape, stone-powder content and clay-lump content. Visually inspect every truck and do not unload nonconforming material. Also test the required properties by batch in accordance with the applicable specifications. For fine aggregates, control fineness modulus, mud content and clay-lump content. Visually inspect every truck and reject unloading if the material is nonconforming; likewise, conduct batch testing as specified.

 

18. Why should coarse aggregate size be controlled within 5–25 mm?

Coarse aggregate size is limited by the diameter of the concrete delivery pipe and the pumping height. In general, the maximum pumpable aggregate size decreases as pumping height increases.

For example, at pumping heights below 50 m, the ratio of maximum coarse aggregate size to delivery-pipe diameter should not exceed 1:3. At a pumping height of 100 m, this ratio falls to 1:5; otherwise, blockages are likely.

 

19. Why must flaky and elongated coarse particles be controlled in pumped concrete?

When their content is high, elongated coarse particles have relatively low flexural strength and bonding between coarse aggregate particles is reduced, lowering concrete strength. In ready-mixed concrete, a high flaky and elongated particle content also means poorer aggregate shape, reducing flowability. Such particles can readily block the pipeline, causing pump blockages or even pipe bursts. Therefore, their content in pumped concrete must be no more than 10%, with stricter requirements for high-strength concrete.

 

20. What type of sand is needed for ready-mixed concrete?

Ready-mixed concrete requires medium sand. In addition to meeting specification requirements for grading, mud content and clay-lump content, at least 15% of the sand should pass the 0.315 mm sieve. This has a major effect on pumpability: too little passing this sieve can cause pump blockages, poor water retention and bleeding.

 

21. What happens when sand is too fine?

If sand is too fine, concrete water demand increases. Concrete made with fine sand has very poor pumpability and workability retention, lower strength, and a greater tendency to crack.

 

22. What can be done when only fine sand is available?

If the sand supply is problematic, fine sand can be blended with some manufactured sand to produce pumped concrete. For example, fine sand with a fineness modulus below 2.0 can be blended with manufactured sand having a fineness modulus of 3.0–3.2, at an approximate ratio of 6:4. Observe flowability and pumpability, and determine the actual proportions through testing.

 

23. What are the consequences of a high mud content in sand?

A high mud content in sand increases concrete water demand, reduces workability retention, increases shrinkage, lowers strength, and makes the structure prone to cracking. Therefore, sand mud content should be controlled to no more than 3% for C30–C50 concrete, with stricter requirements for high-strength concrete.

 

24. Why should smaller coarse aggregates be used in high-strength concrete?

As coarse aggregate size increases, its bond with the cement paste weakens and internal discontinuities increase, reducing concrete strength. Coarse aggregates restrain cement shrinkage in concrete. Because their elastic modulus differs from that of the cement paste, tensile stresses develop internally. These stresses increase with aggregate size and can reduce strength. As aggregate size increases, calcium hydroxide, Ca(OH)₂, crystals become more strongly oriented in the interfacial transition zone, weakening the interface and reducing concrete strength.

Tests show that, around coarse aggregate particles measuring 15–25 mm, interfacial cracks are about 0.1 mm wide and extend over two-thirds of the particle circumference, with more connections to cracks in the surrounding cement paste. Around 5–10 mm particles, interfacial crack widths are more uniform at only 0.03 mm, and crack lengths are only one-sixth of the particle circumference. The amount of water accumulating in pockets beneath coarse aggregate particles during hardening also varies with particle size. Larger particles have more and larger water pockets beneath them. When this water evaporates, wider cracks inevitably form at their lower interfaces than beneath smaller particles, resulting in lower interfacial strength.

 

25. Why can pebble-aggregate concrete have 3–4 MPa lower strength than crushed-stone concrete with the same mix proportions?

A rough coarse-aggregate surface benefits the strength of the interface between cement paste and aggregate.

Based on the author’s many years of testing, pebbles contain more weathered particles and have a lower crushing index than crushed stone. Their smooth surfaces also provide lower interfacial strength. Consequently, concrete made with pebbles has 3–4 MPa lower strength than concrete made with crushed stone at the same mix proportions.

 

26. Why should sand and aggregate moisture content be measured every shift?

Sand and coarse aggregates are each typically used at 800–1,100 kg/m³ in ready-mixed concrete. Each 1% of moisture content therefore changes the water introduced into the concrete by 8–11 kg. Sand, in particular, is often collected from rivers and can have highly variable moisture content. Without frequent moisture testing and timely adjustments to mixing-water quantities, slump, pumpability and strength can fluctuate substantially between batches.

 

27. How does concrete cracking affect a structure?

Cracking affects structural integrity;

Cracking can cause durability problems;

Cracking can lead to a loss of serviceability;

Cracking is aesthetically unacceptable.

28. What are the main factors affecting concrete strength, and how do they affect it?

The main factors affecting concrete compressive strength are:

Cement strength class and water-to-cement ratio. A higher cement strength class produces higher concrete strength. Provided the concrete can be fully compacted, a lower water-to-cement ratio produces higher strength.

Curing temperature and humidity. These affect strength by influencing cement hydration, setting and hardening. With suitable temperatures and high humidity, strength develops rapidly; unfavorable conditions hinder strength development.

Age. Longer curing allows more complete hydration, lower porosity and higher concrete strength.

Construction methods. These mainly refer to mixing, vibration and molding. More effective mechanical mixing and vibratory compaction produce higher concrete strength.

 

29. What basic requirements should be considered when proportioning concrete?

The following four basic requirements should be considered when proportioning concrete:

Meet the strength grade required by the structural design;

Provide the workability required for construction;

Meet durability requirements for the project’s exposure environment;

Follow economic principles by conserving cement to reduce concrete cost.

30. Why must workers be strictly prohibited from adding water arbitrarily to concrete during site placement? Explain the harm in theoretical terms.

When workers add water to the concrete mix during placement, the extra water increases flowability but reduces cohesion and water retention. In particular, the higher water-to-cement ratio, W/C, increases capillary porosity within the concrete, reducing strength and durability and increasing deformation, which can cause quality failures.

Therefore, workers must be strictly prohibited from adding water arbitrarily to the concrete mix during site placement.